Study with the several resources on Docsity
Earn points by helping other students or get them with a premium plan
Prepare for your exams
Study with the several resources on Docsity
Earn points to download
Earn points by helping other students or get them with a premium plan
Community
Ask the community for help and clear up your study doubts
Discover the best universities in your country according to Docsity users
Free resources
Download our free guides on studying techniques, anxiety management strategies, and thesis advice from Docsity tutors
WPS for steel A527 Cl2, SMAW process, Electrode E8016-H2
Typology: Assignments
1 / 3
This page cannot be seen from the preview
Don't miss anything!
1
Date:
Date: Date:
Company Name HAN XUYEN VIET TRADING SERVICES PRODUCTION CO.,LTD
WPS No. HXV-WPS-GT-001 Date: 01, Oct. 2024
Supporting PQR No. (s) HXV-PQR-GT-
Revision No. 0 Date: -
Welding Process(es) GTAW Type(s) Manual
Application Code ASME SECTION IX 2023 Ed. (Automatic, Manual, Machine, or Semi-Automatic)
JOINTS (QW-402)
Joint Design Groove and Fillet Weld (Plate & Pipe)
A
ND OTHER JOINTS DETAIL IN DWG
Retainer None
Root Spacing 3.1±1.6mm w/Back gouging, 5±1mm With backing
Backing With/ without backing
Backing Material (Type) None
( Refer to both backing and retainers)
Metal Nonfusing Metal
Nonmetallic Other
Sketchers, Production Drawing, Weld Symbols or Written Description should show the
general arrangement of the part to be weld. Where applicable, the details of the weld groove
may be specified.
Sketcher may be attached to illustrate joint design, weld layers and bead sequence (e.g.,
for toughness procedure, for multiple process procedures, etc.)
BASE METALS (QW-403)
P-No. 8 Group No. 1 to P-No 8 Group No 1
or
Specification type and grade TP 304 or Equivalent (ASTM A312)
to Specification type and grade TP 304 or Equivalent (ASTM A312)
or
Chem. Analysis and Mech. Prop -
to Chem. Analysis and Mech. Prop -
Thichness Range:
Base Metal: Groove: 1.5 mm ÷ 5.54 mm Fillet: All
Pipe Diameter: All diameter
Maximum Pass Thickness 1/2in.(13mm) Yes No
Other:
*FILLER METALS (QW-404) GTAW
Spec. No (SFA) A 5.
AWS No (Class) ER308L
F-No 6
A-No 8
Size of Filler Metals 2.4 mm
Filler Metal Product Form Solid Rod
Supplemental Filler Metal -
Weld Metals Thinkness Range
Groove Max: 5.54mm
Fillet All size, thickness and diameter
Electrode-Flux (class) N/A
Flux Designnation N/A
Flux Type N/A
Alloy Flux N/A
Flux Trade Name N/A
Consumable Insert N/A
Other N/A
*Each base metal-filler metal combination should be specified individually